Resources / FPC stack-up and layer construction
Design

FPC stack-up and layer construction.

An FPC stack-up is the ordered list of layers that make up a flex circuit, with the thickness of each one: base film, copper, bond, coverlay and any stiffener. It sets the electrical behaviour of the circuit and, just as important, how tightly the finished part can bend.

Two flex circuits built from the same schematic can behave very differently once the stack changes. The stack is the first thing we fix on a new job, before layout, because it decides thickness, bend radius, impedance and cost at the same time.

What is in an FPC stack-up?

A single-sided flex has five things in it, counted from the bottom up. The table gives the thicknesses we work with most often.

LayerTypical thicknessWhat it sets
Polyimide base film12.5, 25 or 50 umFlexibility, dielectric, temperature resistance
Bond to the copperAcrylic 12.5 to 25 um, or noneTotal thickness, registration, heat performance
Copper, RA or ED18, 35 or 70 um (1/2, 1, 2 oz)Current capacity, fatigue life, minimum line width
Coverlay: polyimide plus adhesive12.5 or 25 um film, 15 to 25 um adhesiveInsulation, protection over the bend
Stiffener, local onlyPI 0.1 to 0.25 mm, FR-4 0.2 to 1.6 mm, steel 0.1 to 0.3 mmFlatness under connectors and parts

Add copper on the second face and you have a double-sided flex, joined by plated holes. Bond two of those together and you have a four-layer flex.

How thick is each construction?

Finished thickness is what the bend radius is calculated from, so it is worth knowing before the mechanical design is frozen.

ConstructionCopper layersTypical finished thickness
Single-sided flex10.08 to 0.15 mm
Double-sided flex20.15 to 0.25 mm
Multilayer flex3 to 80.3 mm and up

The pattern is simple. Every copper layer you add makes the stack thicker and stiffer, and the minimum radius grows with it, which is why a multilayer flex normally drops to one or two layers in the zone that folds. The multipliers are in bend radius and flex life.

Adhesive or adhesiveless laminate?

Adhesive-based laminate bonds the copper to the film with a layer of acrylic. It is cheaper and perfectly good for simple one and two layer work. Adhesiveless laminate puts the copper straight onto the polyimide.

We specify adhesiveless when any of three things is true: the part is multilayer, the assembly sees lead-free reflow more than once, or the lines are fine enough that registration through lamination matters. The acrylic layer is the softest thing in the stack, so removing it thins the part, holds dimensions better through heat, and takes out the layer most likely to flow at high temperature.

Where does the copper sit in the bend?

When a flex bends, the outer surface stretches and the inner one compresses. Between them is a plane that does neither, the neutral axis, and copper placed on or near it sees the least strain. That is the whole argument for a symmetric stack: on a double-sided dynamic flex, balancing the two copper layers about the centre is what lets it keep bending without cracking.

It also explains a failure we see on other people’s drawings. Put a thick stiffener or a heavy coverlay on one face only, in or next to the bend, and the neutral axis moves out of the copper. The part then cracks at the edge of that stiffener, not in the middle of the fold.

How do you choose copper weight?

Start from current and line width, then check the bend. Half-ounce copper etches finer lines and bends better. Two-ounce copper carries far more current and is normal on a busbar FPC, but it makes a stiff part that belongs in a static zone. Where a design needs both, we split the functions across the stack rather than compromising on one weight.

From our flex line: The stack-up we quote is not always the one the drawing asks for. The most common change we propose is dropping the bend zone from two copper layers to one and moving the second layer’s routing around the fold, which usually costs a little board area and buys back an order of magnitude in flex life.

What is an FPC stack-up?
The ordered set of layers in a flex circuit with their thicknesses: polyimide base, bond, copper, coverlay and any stiffener. It sets impedance, finished thickness and how tightly the part can bend.
How thick is a flexible PCB?
A single-sided flex is typically 0.08 to 0.15 mm finished, a double-sided flex 0.15 to 0.25 mm, and a multilayer flex 0.3 mm and up. Base film, copper weight and coverlay set the exact figure.
What copper thickness is used in flex circuits?
Most work is 18, 35 or 70 um, that is half-ounce, one ounce and two ounce. Lighter copper bends better and etches finer lines; heavier copper carries more current but stiffens the part.
When should I use adhesiveless laminate?
For multilayer builds, for assemblies that see reflow more than once, and for fine lines where registration matters. It removes the acrylic layer, so the stack is thinner and more stable through heat.
Can stiffeners go in the bend area?
No. A stiffener holds the flex flat under connectors and components, and its edge is a step in stiffness where cracks start. Keep stiffeners and their adhesive clear of the fold.

Need a stack-up reviewed?

Send your flex drawing and we will confirm the stack-up, with feasibility and an indicative price in two working days.