PI
Polyimide base film
RA
Rolled copper for dynamic
0-glue
Adhesiveless option
150°C
Continuous, on polyimide
Why materials decide it

Why do FPC materials decide flex life and cost?

A flexible PCB is built from a polyimide base film, copper foil, a bond system, a polyimide coverlay and stiffeners. Every one of those choices sets how many times the circuit can bend, how thin it is, how hot it can run and what it costs.

Get the material stack right and a flex lasts the life of the product. Get it wrong, with the cheap copper on the moving part or the wrong film for the heat, and it cracks in the field. The rest of this page is how we choose each layer. Where the flex also needs an EMI shield, that film is one more layer in the stack, covered in our flex PCB EMI shielding guide.

The layers of a flex stack.

Each layer is a choice, not a default.

Polyimide base film - I-Tech
Base film

Polyimide vs PET

PI for heat and dynamic flex; PET for low-cost static designs.

Rolled annealed copper foil - I-Tech
Copper

RA vs ED

Rolled annealed survives bending; ED is lower cost for static.

Adhesiveless laminate - I-Tech
Bond

Adhesive vs adhesiveless

Adhesiveless is thinner and more stable through heat.

Polyimide coverlay - I-Tech
Coverlay

Coverlay

Polyimide film that protects the traces where soldermask cannot bend.

Stiffener materials - I-Tech
Stiffener

PI / FR-4 / metal

Rigidity under connectors and components, or for heat spreading.

How we choose each layer.

The default and the reason to change it.

Base film
PI / PET / LCP

PI for heat and dynamic flex, LCP for high-frequency, PET for low-cost static.

Copper type
RA / ED / HA

RA (12 to 70 µm) on anything that moves; ED for static to save cost.

Copper weight
1/2 to 6 oz

1/2 to 2 oz for signal, heavy copper for busbar current.

Bond
Adhesiveless

For high temp, fine lines and multilayer; adhesive for standard builds.

Coverlay
PI, 1/2 to 2 mil

Openings set back from the bend so solder does not stiffen it.

Stiffener
PI / FR-4 / Al / SUS

PI at ZIF tails, FR-4 under parts, metal for strength and heat.

Finish
ENIG / Tin / OSP / Au

ENIG for fine pitch and contact, gold for wear, immersion tin for flat solderable pads, OSP for lowest cost.

Adhesive
Acrylic / epoxy

Acrylic for flexibility, epoxy for temperature and stiffness.

From our flex line

Where adhesiveless earns its cost.

The acrylic adhesive in a standard flex is the softest, most thermally active layer in the stack. On high-temperature or multilayer work it expands, pushes on plated holes and moves the layers out of registration. Adhesiveless laminate removes that layer, so the copper sits straight on the polyimide.

That is why we specify adhesiveless for reflow-heavy assemblies, fine-line designs and any multilayer flex, and keep adhesive-based material for standard single and double-sided builds where its lower cost is the better trade. How that laminate then moves through drilling, imaging, coverlay and test is set out step by step in our flex PCB manufacturing process guide.

High tempAdhesiveless for reflow and service heat
Fine linesStraighter copper, better yield
MultilayerRegistration holds through lamination

Common questions.

What are flexible circuit boards made of?
A flexible PCB is built from a polyimide base film, copper foil, an adhesive or adhesiveless bond, a polyimide coverlay over the traces, and stiffeners where rigidity is needed. Each choice sets the flex life, thickness and cost.
Polyimide or PET for the base film?
Polyimide handles high temperature and dynamic flexing and is the default for reliable flex. PET is cheaper and suits low-cost, low-temperature, static designs, but it cannot take reflow soldering.
What is the difference between RA and ED copper?
Rolled annealed (RA) copper has an elongated grain that survives repeated bending, so it is used for dynamic flex. Electro-deposited (ED) copper is lower cost and fine for static designs that bend once.
What is adhesiveless laminate?
Adhesiveless laminate bonds the copper directly to the polyimide without an acrylic adhesive layer. It is thinner and more stable through heat, which improves high-temperature performance, fine-line yield and multilayer registration.